製品テスト
T bending machine |
塗膜と基材の曲げ特性の試験。試験基準:ひび割れ、塗装、粉のないテープで貼り付ける。 |
Weight impact tester |
Test the adhesion between the coating and the substrate and the toughness of the paint film. |
Thickness gauge |
Check the film thickness of the coating |
Gloss meter |
The degree to which the surface of the object represented by the number is close to the mirror surface mainly depends on the illumination of the light source and the angle of observation; below 45 degrees is matte, 45-60 degrees is semi-high light, and above 60 degrees is high light. |
MEK wipe |
Solvent resistance, to detect the degree of cure of the paint coating |
Hundred Lattice Experiments |
To test the interlayer adhesion between the coating and the substrate inspection. |
Compound experiment |
Detect the cleaning effect of the cleaning line Aluminum-plastic panel: use the tension-indicating reagent to test, and the plain paint “37” is horizontally wiped, and the shrinkage time of the reagent is more than 10 seconds. The silver paint is wiped horizontally with the “37” reagent, and the shrinkage time of the test machine is more than 5 seconds. |
Boiling experiment |
Detect the adhesion between the coating and the substrate layer. |
Pencil hardness test |
Test the hardness index of the paint film. The length of the pencil lead is 3CM, put it on a flat surface with sandpaper, and grind the pencil lead vertically with the surface of the sandpaper to keep the mark far sharp. The pencil and the sample are pushed forward at a constant speed at an angle of 15 degrees, and pencils with different hardnesses are used to make 5 strokes. Check the scratches on the surface of the paint film to confirm the measured value. |
Protective film tensile tester |
Test the viscosity of the finished protective film. Plain paint: 8N-10N Silver paint: 10N-15N. The 10cm protective film is compacted by a laminating machine on a matte standard base plate with a width of 10cm, and then a tension machine is used at 2cm/sec. The speed is 180 degrees horizontally and uniformly peeled off, and the displayed value is the viscosity of the protective film |
Micrometer |
The micrometer is zeroed and measured 3 times at different positions and averaged (the maximum deviation between the 3 measured values shall not exceed the error range). The maximum deviation or the total thickness exceeding the standard shall be regarded as unqualified. |
Salt spray test |
Simulate the environment of the ocean or the climate of the salty and humid area to test the salt spray corrosion resistance of the finished product. The assay used 5% sodium chloride. Our testing time is generally 2000 hours, which is equivalent to 6 years in a humid and corrosive environment at the seaside |
Weathering test machine |
Simulate changes in the climate and environment by ultraviolet rays, temperature, humidity (condensation) in sunlight, detect the aging degree of products and materials in a short period of time, and reflect the phenomenon of discoloration and fading of product coatings. |